Polyurethane Self Levelling

Polyurethane Self Levelling

Two-component, self-leveling, waterproof, chemical and
It is resistant to abrasion and used to add flexibility to the floor.
It is a coating material.

Characteristic Features                      

Colour                                                                                                 in various colors

Density of the mixture                                                 1.40kg/L

Viscosity(20oC)                                                                     1200cP

Mixing ratio                                                                         18:4 

Curing time                                                             6-8 hours (25°C)

heat resistance                                                               100 °C (For cured product)  
Shore A                                                                                             80 ±5 

Application time                                                             15-45 min.

(Varies depending on humidity and temperature  
shows.)

Surface Preparation                                                                   The floor is clean, dry, free of oil and dust  
must be purified.

Touch Dry                                                 6-8 hours

Application Procedure                                                  Polyurethane self leveling 4.5 by weight  
1 part component A with 1 part component B  
It is obtained by mixing. It should be mixed with a slow speed mixer for at least 2 minutes. Care should be taken to ensure that the two components are thoroughly mixed.  Let the mixed material sit for 15-45 minutes.  It must have been used inside.  It varies depending on the air temperature. A squeegee or trowel should be used for application. Application temperature should be between 10° C - 30° C.

Technical Documents

Technical documents are not available for direct download. Leave your details and we will email the document.